Crystallization regulation of Fe<sup>0</sup>@Fe<sub>3</sub>O<sub>4</sub> using a g-C<sub>3</sub>N<sub>4</sub>/diatomite composite for enhancing photocatalytic peroxymonosulfate activation

Figure 2. SEM images of (A) diatomite, (B) Fe0@Fe3O4, (C and D) 0.6-FNGD and (E) SEM-EDS elemental mapping of Si, C, N and Fe for 0.6-FNGD composite.